(1) Loose mold: The movement of the punch or mold exceeds the unilateral gap. Adjust the combination gap.
(2) Die inclination: The straightness of the die or die is not correct, or there are foreign objects between the templates, making it impossible for the templates to be flat. Reassemble or grind for correction.
(3) Template deformation: Insufficient hardness or thickness of the template, or deformation caused by external impact. Replace with a new template or correct the disassembly method.
(4) Mold seat deformation: Insufficient thickness or uneven force on the mold seat, resulting in variations in the straightness of the guide pillar and guide sleeve. Grind, correct, or refill plastic steel, or replace the mold seat or evenly distribute the force.
(5) Die interference: Check whether the size and position of the die are correct, whether there is any deviation in the positioning of the upper and lower dies, whether there will be looseness after assembly, and whether the accuracy of the punching machine is not high and the die is not upright.
(6) Punch shear deviation: The punch strength is not enough, the size of the punch is too close, the lateral force is not balanced, and the punch is half inclined. Strengthen the guidance and protection function of the stripping inclined plate, or increase the punch size or shorten the small punch to increase the heel length and support early guidance, paying attention to the feeding length.